A fitness retailer ordering EVA yoga blocks rarely receives one SKU at a time. The purchase order may cover single blocks sold on their own and two-packs bundled for home-studio shoppers, packed in different carton configurations but moulded from the same batch of high-density EVA foam. That is exactly where a receiving inspection goes wrong: the team checks quantity and carton condition, signs for the shipment, and only discovers weeks later that one block size crushes under a shopper's weight while the other springs back. This guide explains what compression recovery under load means, how to record it at goods receipt, and how to keep the record comparable when single units and two-packs arrive in the same delivery.
Compression recovery describes what a foam block does after a load sits on it and is then removed: does it return to its original height, or does it stay permanently flattened? A block that stays flattened has lost the support it was bought to provide. Blocks are used to support stretching and balancing poses, so a shrunken block changes how a pose is held and where the practitioner's weight ends up.
The reason to test at goods receipt rather than in the showroom is comparability. Blocks shipped loose, blocks shrink-bagged as singles, and two blocks packed face to face in one retail sleeve all travel differently. Corrugated cartons soften over a long ocean passage, and stacked pallets put static load on the lowest cartons for weeks. Testing while the paperwork is still open lets you tie every reading to a specific carton, so a soft block can be traced to how it was packed rather than blamed on the foam in general.
Fulikai's yoga blocks are moulded from high-density EVA foam and described as firm yet comfortable and resistant to deformation, with smooth rounded edges and a non-slip surface. The published specification is 3 × 6 × 9 inches, with one piece per shrink bag. The same product page states that the blocks keep their shape under heavy weight and can support a person whether standing or sitting on them.
Two points matter for the inspection record. First, the listed packaging unit is one piece per shrink bag, so any two-pack your retailer plan requires is a packing decision made at order stage, not something implied by the base specification. Confirm it in writing before production, because it changes both the carton layout and the number of blocks exposed to edge load in transit. Second, the size figure belongs to the block, not to the bag or the retail sleeve; measure the block itself when you record a reading.
A usable record answers three separate questions. Keep them in three columns so a reviewer can see which stage failed.
| Reading | What you are checking | How to take it at the dock |
|---|---|---|
| Free height | Whether the block arrived already compressed after transit loading | Let the block rest flat on a hard table away from the stack, then measure its height across the 3-inch dimension at several points along the length |
| Deflection under load | How far the block sinks while a load is held on it | Place the block flat, put a known weight on the centre of the top face, wait for the height to settle, and record the loaded height |
| Recovered height | Whether the foam returns after the load is removed | Remove the weight, let the block rest, re-measure, and compare with free height |
Record each reading as a number plus the conditions around it: the load used, how long the load was held, how long the block rested afterwards, the ambient temperature in the receiving area, and the batch or carton the block came from. A height figure with no conditions attached cannot be compared against next season's order.
The comparison only means something if both formats are sampled the same way. Before opening cartons, write down how each format was packed and where it sat in the stack, because that is the variable most likely to explain a difference between them.
If the two-pack samples recover less than the singles, the first explanation to rule out is packing pressure, not foam quality. If both formats recover poorly and the readings are spread across cartons and pallet positions, the pattern points back to material or moulding, and that is a conversation for the factory rather than the freight forwarder.
Most receiving disputes fail because nobody agreed in advance what a passing block looks like. Before the order is placed, set out on the purchase order: the load to be applied, how long it is held, the rest period before the recovered-height reading, and the maximum permanent change you will accept. Then attach the completed dock sheet to the receipt as part of the delivery record.
Ask the manufacturer for its own test data on the same block at the same load, and check whether their method matches yours. If they hold a batch report at a different load or holding time, your numbers are not directly comparable, and you will spend the dispute arguing about method instead of foam.
Fulikai operates a Shenzhen factory of over 3,000 square metres with production lines for foaming, cutting, stamping and laser processing, and states that products pass 16 types of test during production, covering areas such as colour fastness, tensile strength and children's product safety. The company also describes full manual inspection before shipment, support for third-party inspection, and factory audit reports from Coca-Cola, Walmart and Sedex. Its Custom Capabilities page lists ISO 9001:2015 together with CE, EN-71, FDA, FCC, RoHS, SGS and REACH, while the About Us page cites an earlier ISO 9001 revision; ask which certificate or test report applies to your market and to this specific block before you rely on any compliance claim in your own listing.
As an OEM and ODM EVA foam manufacturer, Fulikai also produces related studio items such as the EVA yoga mat in TPE/EVA, which retailers often order alongside blocks. Blocks and mats come from different material setups, so keep their receiving checks separate rather than assuming one passes the other.
For each sampled block record: sample ID and carton number; pallet position; format (single or two-pack); free height at several points; applied load and holding time; loaded height; rest period; recovered height; permanent change from free height; edge and surface condition; inspector name and date. Keep the physical sample in its original packaging until the claim window closes.
Two habits make the sheet worth more than the paper it is printed on. Write the numbers as you take them instead of reconstructing them at the end of the shift, and photograph any block whose recovered height falls outside your limit with the carton label visible in the frame. That single photo turns a vague complaint about soft blocks into an evidence-backed claim against a specific case.
For questions on block specification, packing format or inspection arrangements, contact Shenzhen Fulikai Packaging Products Co., Ltd. by phone at +86 13827489472 or by email at sales@fulikaisz.com.cn, or send an enquiry through the message page.